ScrapBull
Marketplace/Ferrous/#2 Heavy Melting Steel
#2 Heavy Melting Steel
Ferrous

#2 Heavy Melting Steel

Grade: 202Medium Tier

Steel scrap under 1/4 inch thickness. Tin plate, sheet steel, light gauge materials

Market Price EstimateUpdated Daily
$380/ MT
-8 (-2.1%)vs yesterday
Verified specifications & market data

Certification Requirements

Required certifications, standards compliance, and verification protocols.

ISO 9001:2015
Scope

Supplier's scrap collection, sorting, baling/compacting, quality control

ISO 14001:2015
Scope
  • Environmental Compliance
  • Oil/Fluid Handling
  • Waste Segregation
WEEE Directive Compliance
Certificate of Analysis
Content
  • Chemical composition (XRF)
  • Sampling methodology
  • Test results vs. specification
  • Inspector signature
Issued By
  • UKAS accredited laboratory
  • ILAC accredited laboratory
Baling/Compacting Equipment Certificate
Insurance Certificate
Minimum Coverage

£2–5 million general liability

Rejection Criteria

Conditions and thresholds that trigger immediate rejection or downgrading.

Copper contamination
Threshold

>0.15%

Action

REJECTION (relaxed vs. HMS #1 which is <0.10%)

Reason
  • Copper >0.15% Affects Eaf Steel Ductility
  • #2 Hms Allows Higher Limit Due To Light Gauge Nature
Test Method

XRF spectrometry

Severity

CRITICAL

Stainless steel mixing
Threshold

>0.1% detected

Action

REJECTION

Reason
  • Austenitic Stainless Degrades Ferrous Steel Quality
  • Indicates Inadequate Sorting
Test Method

XRF + magnetic test

Severity

CRITICAL

Galvanized steel excess
Threshold

>5% by weight (Zn source)

Action

Rejection or credit negotiation based on Zn % verification

Reason
  • Excessive Galvanized Coating Increases Zinc Contamination
  • Reduces Final Steel Properties
Test Method

XRF spectrometry (zinc measurement)

Severity

MAJOR

Non-ferrous contamination
Threshold

>2.5% combined (higher tolerance than HMS #1 at 2.0%)

Action

Rejection or credit adjustment

Reason

Light gauge scrap permits higher non-ferrous tolerance than solid HMS

Test Method

XRF spectrometry

Severity

MAJOR

Moisture content
Threshold

>2% moisture

Action

Re-dry and re-test or rejection

Reason
  • High Moisture In Thin Material
  • Unacceptable For Eaf Melting
Test Method

Karl Fischer titration

Severity

MAJOR

Iron content below minimum
Threshold

Fe <97.5%

Action

REJECTION

Reason

Violates ISRI 202 minimum specification

Test Method

XRF spectrometry

Severity

CRITICAL

Visible copper wire
Threshold

Any visible strands >0.5mm diameter

Action
  • Manual Removal Required
  • Possible Rejection If Excessive
Reason

Copper wire indicates incomplete separation

Test Method

Visual inspection

Severity

MAJOR

Radioactive contamination
Threshold

Any detectable

Action
  • Immediate Rejection
  • Hazmat Protocol
Reason

Health and safety hazard

Test Method

Radiation detector scan

Severity

CRITICAL

PCB or hazardous electronics
Threshold

Any visible

Action
  • Full Rejection
  • Hazardous Waste Protocol
Reason

Environmental and regulatory hazard

Test Method

Visual inspection

Severity

CRITICAL

Asbestos or mercury components
Threshold

Any detectable

Action
  • Full Rejection
  • Hazmat Disposal
Reason
  • Hazardous Materials
  • Health Risk
Test Method

Visual + laboratory analysis if suspected

Severity

CRITICAL

Heavy oil contamination
Threshold

>2% by weight

Action

Cleaning or credit adjustment

Reason

Excess oil contaminates EAF furnace

Severity

MODERATE

Cookie Notice