.jpg&w=3840&q=75)
Ferrous
Busheling Scrap
Grade: 207High Tier
New ferrous scrap from stamping plants, clean, uncoated steel
Market Price EstimateUpdated Daily
$415/ MT
+18 (4.5%)vs yesterday
Verified specifications & market data
Chemical Composition
Elemental breakdown by percentage weight.
Standard composition limits
Values represent maximum allowed percentage unless otherwise noted.
Physical Properties
Material form, density, and contamination specifications.
Clean, uncoated steel trim, slugs, and waste directly from automotive/appliance stamping presses; material flows directly from press to collection with zero weathering
Acceptable Inclusions
- Light press cooling water residue <0.5%
- Dust from metal stamping <0.2%
- Minimal rust from press surface <0.1%
Prohibited Materials
- Coatings: paint, oils, grease (any visible)
- Stainless steel (any piece >0.02%)
- Non-ferrous metals: copper, aluminum, brass, lead (any detectable)
- Radioactive materials (any detectable)
- PCB or electronic components
- Asbestos materials
- Mercury components
- Mixed scrap from collection areas (busheling must be press-direct)
Quality Assurance
Testing protocols, sampling methods, and acceptance criteria.
Sampling Protocol
frequencyRandom selection from multiple bushels; confirms uniformity
maximumQuantity30 samples per truck load
minimumQuantity500kg or 10 samples
percentage3–5% of lot
sourceVerificationMaterial must be verifiable to specific stamping press/facility lot number
Acceptance Limits
all Criteria Must Passcriteria must simultaneously be met; single criterion failure triggers rejection
copper LimitCu <0.05%
iron ContentFe ≥95.0%
non Ferrous Total<1.0%
origin VerificationMaterial must be press-direct; lot tracking required
stainless Limit<0.02%
trace ElementsAll <0.05%
visual Contaminantscontamination visible
Weight Tolerance
notesManufacturing control enables tight variance; precise bushel collection
variance±2% acceptable
Required Test Methods
Visual Inspection
Purpose
- Detect ANY non-ferrous metal pieces, stainless steel, coatings, contamination
Acceptance Criteria
- Pass: ZERO contamination visible
- 100% factory-clean appearance
Procedure
- 100% visual inspection of material samples
- ZERO tolerance for contamination
XRF Spectrometry
Purpose
- Verify Fe ≥95%, Cu <0.05%, non-ferrous <1.0%
Acceptance Criteria
- Pass: Fe ≥95%, Cu <0.05%, non-ferrous <1.0%, all trace elements within limits
Magnetic Test
Purpose
- Confirm ferrous material
- detect any stainless or non-magnetic contamination
Acceptance Criteria
- Pass: All samples respond strongly to magnet
- NO dead zones
Procedure
- Hand magnet test on representative samples
Surface Condition Assessment
Purpose
- Verify material is clean, uncoated, and factory-direct
Acceptance Criteria
- Pass: Appearance confirms manufacturing origin (not weathered, not oxidized)
Procedure
- Visual inspection for rust, oxidation, oil stains, paint, dirt
Material Origin Verification
Purpose
- Confirm material is busheling (press-direct), not mixed scrap
Acceptance Criteria
- Pass: Documentation available
- traceability to specific press/facility
Procedure
- Review supplier documentation
- verify lot tracking number