ScrapBull
Marketplace/Non-Ferrous Brass/New Brass Clippings
New Brass Clippings
Non-Ferrous Brass

New Brass Clippings

Grade: LabelHigh Tier

Clean new brass clippings and stamping scrap

Market Price EstimateUpdated Daily
$2,950/ MT
+155 (5.5%)vs yesterday
Verified specifications & market data

Certification Requirements

Required certifications, standards compliance, and verification protocols.

ISO 9001:2015 Quality Management System
Scope

Brass clipping collection, sorting by alloy, cleanliness verification, packaging, quality control

Requirement

Supplier must maintain active ISO 9001 certification throughout contract term

Certification BodyAccredited third-party audit body
RenewalAnnual audit required; certification must remain current
Certificate of Analysis
Content
  • Copper content: 55-70% confirmed (new brass clipping specification range)
  • Zinc content: 25-40% confirmed (brass alloy component)
  • Lead content: ≤1.0% CONFIRMED (STRICT premium purity specification)
  • Iron content: <0.3% confirmed (ferrous contamination minimal; virgin material)
  • Tin content: <0.2% confirmed (bronze contamination essentially prohibited)
  • Nickel content: <0.1% confirmed (new material purity)
  • Manganese content: <0.2% confirmed (residual alloying minimal)
  • Silicon content: <0.2% confirmed (oxide/silica minimal)
  • Aluminum content: <0.1% confirmed (non-ferrous contamination essentially prohibited)
  • Oxidation level: <1.0% documented (virgin material; light patina only)
  • Oil/coolant residue: <0.5% CONFIRMED (virgin material must be dry/clean)
  • Material origin: NEW/VIRGIN/NEVER-MELTED status EXPLICITLY VERIFIED
  • Cleanliness condition: PRISTINE clean status documented
  • Alloy specification: identified and documented (if sorted by type)
New/Virgin Material Certification
Explicit Requirement

MUST state:

  • Confirmed NEW/VIRGIN BRASS CLIPPINGS
  • material NEVER previously melted
  • direct factory scrap from brass manufacturing
  • original virgin condition preserved
  • never recycled or reprocessed
Lead Content Verification
Explicit Requirement

MUST state:

  • Lead content verified ≤1.0%
  • STRICT premium purity specification confirmed
  • material meets virgin brass clipping premium grade requirements
XRF Elemental Analysis Report
Requirement
  • Complete Elemental Profile Confirming New Brass Clippings Specification
  • Premium Purity Verified
  • Virgin Material Composition Confirmed
ISRI Label Grade Certification
Explicit Requirement

MUST state:

  • New Brass Clippings
  • ISRI Label Grade
  • Cu 55-70%
  • Zn 25-40%
  • Pb ≤1.0%
  • virgin/new material purity verified
  • clean condition confirmed
  • direct mill feedstock quality
Cleanliness & Condition Certificate
Explicit Requirement

MUST state:

  • Material confirmed clean/pristine condition
  • minimal oxidation <1.0%
  • no heavy contamination
  • virgin material character preserved
  • ready for direct mill charge
Oil/Coolant-Free Certification
Explicit Requirement

MUST state:

  • Oil/coolant residue <0.5%
  • material confirmed DRY/CLEAN
  • no machining fluid saturation
  • virgin material processing-free condition
Insurance Certificate
Minimum Coverage
  • Premium Virgin Material
  • High-Value Commodity

Rejection Criteria

Conditions and thresholds that trigger immediate rejection or downgrading.

Material not new
Threshold

Heavy oxidation >2% OR aged appearance OR composition inconsistent with virgin material

Action

FULL REJECTION or reclassification to used/recycled brass grade (-£100-200/MT penalty)

Reason
  • Critical: Premium Grade Requires Virgin/New Material Certification
  • Aged/Recycled Violates Specification
Test Method

Visual oxidation assessment + composition analysis

Severity

CRITICAL - GRADE VIOLATION (ABSOLUTE)

Consequence:
  • Full Rejection Or Substantial Downgrading
  • Material Loses Virgin Premium Status
Copper content out of range
Threshold

Cu <55% OR Cu >70%

Action

Full rejection or major reclassification

Reason

Material not consistent with new brass clipping specification

Test Method

XRF spectrometry

Severity

CRITICAL - SPECIFICATION VIOLATION

Consequence:

Full lot rejection or downgrading to different commodity

Zinc content inconsistent
Threshold

Zn <25% OR Zn >40%

Action

Full rejection or major reclassification

Reason
  • Composition Imbalance
  • Not New Brass Clippings
Test Method

XRF spectrometry

Severity

CRITICAL - SPECIFICATION VIOLATION

Consequence:

Full rejection or substantial downgrading

Lead contamination excessive
Threshold

Pb >1.0% (ANY EXCESS violates strict specification)

Action

AUTOMATIC FULL REJECTION

Reason
  • Critical: Strict ≤1.0% Lead Specification Non-Negotiable
  • Premium Purity Gate Violation
Test Method
  • Xrf Spectrometry
  • Accurate To ±0.1%
Severity

CRITICAL - PREMIUM SPECIFICATION VIOLATION (ABSOLUTE)

Consequence:
  • Full Rejection
  • Material Loses Premium Virgin Status
  • May Reclassify To Standard Brass
Ferrous contamination
Threshold

Fe >0.3% OR magnetic attraction detected

Action

Full rejection or mandatory magnetic separation

Reason
  • Virgin Material Must Be Non-Ferrous
  • Ferrous Contamination Indicates Wrong Material
Test Method

Magnetic test + XRF

Severity

CRITICAL - CONTAMINATION

Consequence:

Full rejection or material segregation/separation mandatory

Stainless steel or aluminum contamination
Threshold

>0.5% stainless OR >0.1% aluminum detected

Action

Full rejection

Reason
  • Non-Ferrous Mixing
  • Wrong Material
  • Virgin Purity Violated
Test Method

XRF spectrometry + visual inspection

Severity

CRITICAL - CONTAMINATION

Consequence:
  • Full Rejection
  • Material Fundamentally Wrong
Oil saturation or hazardous contamination
Threshold

Oil >1% OR hazardous substance detected

Action

Full rejection

Reason
  • Virgin Material Specification Violated
  • Processing Fluid Contamination
  • Hazmat Concern
Test Method

Visual/tactile + loss on heating if necessary

Severity

CRITICAL - SPECIFICATION VIOLATION

Consequence:
  • Full Rejection
  • Material Reclassified Away From Virgin Premium Grade
Heavy oxidation/aged appearance
Threshold

Oxidation >2% OR material visibly aged/tarnished

Action

Full rejection or major reclassification

Reason
  • Indicates Recycled/Aged Material
  • Not Virgin New Condition
Test Method

Visual inspection + oxidation level assessment

Severity

CRITICAL - MATERIAL TYPE VIOLATION

Consequence:

Rejection or -£100-200/MT reclassification penalty

Unknown material or composition
Threshold

Cannot confirm new brass clippings; composition indeterminate

Action

Full rejection

Reason
  • Material Identity Uncertain
  • Must Be Identifiable New Brass Clippings
Test Method

XRF analysis + expert assessment + visual evaluation

Severity

CRITICAL - IDENTIFICATION FAILURE

Consequence:
  • Material Rejected
  • Requires Extensive Testing
Cookie Notice