Stainless Steel 430
Ferritic stainless, magnetic, 16-18% chrome, minimal nickel
Certification Requirements
Required certifications, standards compliance, and verification protocols.
Stainless collection and handling QMS
- Chromium, nickel <0.75% (CRITICAL verification)
- Iron, carbon, sulfur, phosphorus
- Magnetic property confirmation
- Explicit Statement: 'Magnetic (Ferritic)
- Nickel <0.75%
- Grade 430 Confirmed'
£2–3 million general liability
Rejection Criteria
Conditions and thresholds that trigger immediate rejection or downgrading.
NO or weak magnetic response (should be strong)
FULL REJECTION
- 430 Is Strongly Ferritic Magnetic
- No Magnetic Response Indicates 304/316 Contamination
Ni >0.75% (should be <0.75%)
Full rejection or major credit
Ni >0.75% indicates austenitic contamination (304 = 8-10.5%, 316 = 10-14%)
Cr <16.0% OR >18.0%
Full rejection
Grade specification violation
Fe <80% OR >88%
Full rejection
- Ferritic Definition Violation
- Too Much Alloying Indicates Wrong Grade
>0.5% molybdenum
Full rejection
- 430 Has No Molybdenum
- Presence Indicates 316 Contamination
>0.12%
Full rejection or credit
- Ferritic Embrittlement
- Workability Impairment
Evidence of 304, 316, or other austenitic grades
Full rejection
- Ferritic/Austenitic Mixing Compromises Specifications
- Mills Segregate Grades
Any visible or suspected mixing
FULL REJECTION
- Carbon Steel Degrades Stainless Furnace
- Melt Failure
Any detectable
- Immediate Rejection
- Radioactive Waste Protocol
Any visible
- Full Rejection
- Hazardous Waste Protocol
Any detectable
- Full Rejection
- Hazmat Disposal